Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsTribologyAlloysCoatingsCorrosion MechanismsCorrosion ResistanceElectrochemical CorrosionElectrode MaterialsCorrosion Of Nickel-based AlloysCorrosion ProcessesElectrochemical BehaviorElectrochemical MechanismsHeat Treatment EffectsIntermetallic Compound FormationNickel AlloysNickel-based Alloys
This paper describes the effects of heat treatment on the electrochemical behavior and tribological characteristics of Ni-P (10.65 at.% P) composite coatings. The deposits were obtained via electrodeposition onto an AISI 1018 steel electrode and then heat treated at various temperatures ranging from 200 to 600 °C for 60 min in air. The tribological characteristics studied included hardness, friction coefficient, and wear resistance. Polarization curves were used to evaluate the electrochemical behavior (corrosion resistance) of the coatings. The results indicated that the Ni-P alloy (10.6 at.% P) was originally amorphous and was transformed into a mixture of amorphous and crystalline phases when was thermally treated in the range from 400 to 500 °C. This phase transformation was associated to with the precipitation of a mixture of Ni3P intermetallic compound and pure Ni crystals. In addition, the results showed that the wear resistance of the Ni-P coating (10.6 at.% P) increased with hardness. The maximum hardness (990 Hv) was obtained when the Ni-P coatings (10.6 at.% P) were thermally treated at 500 °C. The corrosion current density of the coatings also increased with increasing annealing temperature.
28
Wear behavior of Ni–P and Ni–P–Al2O3 electroless coatings
S. Alirezaei, S. M. Monirvaghefi, Mehdi Salehi et al. · Wear · 2006 · 182 citations