International Journal of Electrochemical Science · 2015 · 15 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceElectrochemistryMetallic MaterialsSurface ScienceAlloysCoatingsElectrochemical TreatmentElectrode MaterialsMetalsSurface CoatingsCurrent DensityCurrent EfficiencyElectrochemical Deposition CoatingsElectroplated CoatingsGrain StructureHardnessNickel AlloysNickel-based Alloys
Ni-Co alloy coatings were deposited to copper substrate electrochemically from a sulphate bath. An increase of cobalt sulphate concentration in the electrolyte from 20 g.l-1 to 45 g.l-1 resulted in a gradual increase in the content of cobalt in the alloy coating from 31.8 wt% Co up to 49.2 wt% Co [1,2]. Ni-Co alloy coatings were deposited at various current densities, namely, 1, 2, 4 and 6 A.dm-2. The values of the current efficiency were achieved in the range of 90 - 98.5 %, when increase of current density led to decrease in current efficiency of process [3,4]. Morphology and grain size of alloy coatings are greatly affected by Co content and current density of process. By increasing Co content, surface morphology of alloy coatings had a finer grain structure. The relationship between concentration of Co in the coating and in the sulphate bath, and the HV0.1 hardness of the deposited coating was shown that the highest value of hardness, 556.3 HV0.1 was measured for coating with 42.6 % Co and concentration of 30 g.l-1 CoSO4 in sulphate bath.
11
Influence of pH on the electrolytic deposition of Ni–Co films
Renáta Oriňáková, Andrej Oriňák, Guido Vering et al. · Thin Solid Films · 2008 · 74 citations
Natural Sciences, Materials Engineering, Materials Science +14