Natural SciencesMaterials EngineeringMaterials ScienceElectrochemistryEnergy MaterialsMaterials ChemistryBattery MaterialsBattery TechnologyElectrochemical Energy StorageElectrode MaterialsEnergy StorageEnergy Storage MaterialsBattery Electrode MaterialsBinder SystemsEnergy Storage ElectrodesFailure MechanismsLithium-ion BatteriesLithium-ion Battery MaterialsSiliconSpecific Capacity
State of-the-art Si electrodes for Li-ion batteries typically require the addition of an advanced polymeric binder and a conductive carbon additive to the active material in order to circumvolve the issues associated with silicon, namely its poor conductivity in the oxidized state, and its high volume variation upon lithiation which give rise to several failure mechanisms. Here, we demonstrate that both additives can be replaced by a cheap, naturally available, polyphenol, tannic acid (TA). We show that Si/TA electrodes (80/20 wt%), even with a high loading (∼2 mg_Si cm−2), can retain a specific capacity above 2000 mAh g−1 after 50 cycles. This unexpected result appears to result from the irreversible reduction of TA during the first cycle, into a conducting, likely polymeric, species.
29
Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
Shan Huang, Scott X. Mao, Ting Zhu · ACS Nano · 2012 · 2.3K citations
Nikolaus Hochgatterer, Mario Schweiger, Stefan Koller et al. · Electrochemical and Solid-State Letters · 2008 · 439 citations
Natural Sciences, Materials Engineering, Materials Science +17