The high temperature oxidation and thermal shock behavior of a dense WSi2–TaSi2 coating on Ta substrate prepared by a novel two-step process

Lairong Xiao, Yuxiang Xiao, Xiao‐Jun Zhao, Xiaojun Zhou, Gang Zhao, Qi Zhong, Huali Yu, Sen Wang, Zhenwu Peng, Zhenyang Cai

Ceramics International · 2023 · 10 citations · 48 references

DOIFull text

Open access

Concepts

Abstract

In order to improve the oxidation resistance of the Ta substrate, a novel two-step process including molten salt electrodeposition (Na 2 WO 4 -WO 3 system) and halide activated pack cementation was adopted to prepare a WSi 2 –TaSi 2 coating on tantalum substrate. During the electrodeposition process, dense tungsten coatings were fabricated at current densities of 30 mA/cm 2 , 40 mA/cm 2 and 50 mA/cm 2 . It was observed that the grain size exhibited a log-normal distribution. When the current density was 40 mA/cm 2 , the grain size and flattest surface of the tungsten coating reached 9.50 ± 0.23 μm and 6.792 μm, respectively. When performing the static oxidation test, the WSi 2 –TaSi 2 coating could effectively protect the Ta substrate oxidized at 1600 °C for 30 h. This is attributed to the presence of dense SiO 2 and Ta 2 O 5 , which acted as a protective layer and suppressed the further penetration of oxygen. Furthermore, due to the matching thermal expansion coefficient between each layer and the sealing ability of semi-molten SiO 2 , the four-layer SiO 2 –W 5 Si 3 –WSi 2 –Ta 5 Si 3 coating could successfully pass 721 thermal shock tests from 1600 °C to room temperature.

References

48