Materials · 2023 · 16 citations · 17 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsMetallurgyAlloysGrain Structure FormationMetal MaterialsMetalsMicrostructure AnalysisMicrostructure EvolutionAluminium AlloysAluminum AlloysHardening ResponseMetal MicrostructureMetallurgical Microstructure AnalysisPrecipitation HardeningPrecipitation-hardening ResponseYield Strength
The aim of this study was to investigate the impact of the addition of a minor quantity of Si on the microstructure evolution, heat treatment response, and mechanical properties of the Al–4.5Cu–0.15Ti–3.0Mg alloy. The microstructure analysis of the base alloy revealed the presence of α-Al grains, eutectic α-Al-Al2CuMg (S) phases, and Mg32(Al, Cu)49 (T) phases within the Al grains. In contrast, the Si-added alloy featured the eutectic α-Al-Mg2Si phases, eutectic α-Al-S-Mg2Si, and Ti-Si-based intermetallic compounds in addition to the aforementioned phases. The study found that the Si-added alloy had a greater quantity of T phase in comparison to the base alloy, which was attributed to the promotion of T phase precipitation facilitated by the inclusion of Si. Additionally, Si facilitated the formation of S phase during aging treatment, thereby accelerating the precipitation-hardening response of the Si-added alloy. The as-cast temper of the base alloy displayed a yield strength of roughly 153 MPa, which increased to 170 MPa in the Si-added alloy. As a result of the aging treatment, both alloys exhibited a notable increase in tensile strength, which was ascribed to the precipitation of S phases. In the T6 temper, the base alloy exhibited a yield strength of 270 MPa, while the Si-added alloy exhibited a significantly higher yield strength of 324 MPa. This novel Si-added alloy demonstrated superior tensile properties compared to many commercially available high-Mg-added Al–Cu–Mg alloys, making it a potential replacement for such alloys in various applications within the aerospace and automotive industries.
17
Two types of S phase precipitates in Al–Cu–Mg alloys
S.C. Wang, M.J. Starink · Acta Materialia · 2006 · 333 citations
Natural Sciences, Materials Engineering, Materials Science +12
Hot tearing mechanisms of B206 aluminum–copper alloy
F. D’Elia, C. Ravindran, D. Sediako et al. · Materials & Design (1980-2015) · 2014 · 63 citations