Science and Technology of Welding & Joining · 2022 · 13 citations · 19 references
EngineeringMaterials EngineeringMaterials ScienceMetallic MaterialsMetallurgyStructural MaterialsAlloysLaser Beam WeldingMetalsSolidification CrackingWeldingWelding ProcessesCracking SusceptibilityLiquation CrackingMulti-pass WeldingRepair WeldingSingle-mode LasersWeld TestingWeldability Of AlloysWelding Metallurgy
The liquation cracking temperature range (LCTR) of CM247LC was evaluated, especially in remelted and reheated weld metals produced during multi-pass repair welding. The LCTR of the remelted weld metal was 282 K, and those of the reheated weld metals were 455–805 K depending on the testing position. In the multi-bead within the reheated weld metal, the LCTR increased from 455 K far from the inter-pass boundary to 805 K near this boundary. The mechanism underlying the varying LCTR for the remelted and reheated weld metals was the amount of MC carbide at each weld position. The single-mode fibre laser welding suppressed the carbide within both areas, and lowered the liquation cracking susceptibility.
19
Guillaume Bidron, Anis Doghri, T. Malot et al. · Journal of Materials Processing Technology · 2019 · 110 citations · Full text