Polymers · 2022 · 24 citations · 24 references
Natural SciencesMaterials EngineeringMaterials ScienceNanomaterialsNanotechnologyPolymer MaterialsHybrid NanomaterialsNanomaterial CharacterizationPolymer CharacterizationPolymer NanocompositesPolymer Phase BehaviorPolymer Thin FilmsFrictionNanocomposite FilmsNanofillersNanoscale TribologyNanostructured Polymer FilmsOrganic-inorganic NanocompositesPolymer Surface ChemistrySpherulitic Morphology
The solvent casting method was used for five types of polyvinylidene difluoride (PVDF) nanocomposite film preparation. The effect of nanofillers in PVDF nanocomposite films on the structural, phase, and friction and mechanical properties was examined and compared with that of the natural PVDF film. The surface topography of PVDF nanocomposite films was investigated using a scanning electron microscope (SEM) and correlative imaging (CPEM, combinate AFM and SEM). A selection of 2D CPEM images was used for a detailed study of the spherulitic morphologies (grains size around 6–10 μm) and surface roughness (value of 50–68 nm). The chemical interactions were evaluated by Fourier transform infrared spectroscopy (FTIR). Dominant polar γ-phase in the original PVDF, PVDF_ZnO and PVDF_ZnO/V, the most stable non-polar α-phase in the PVDF_V_CH nanocomposite film and mixture of γ and α phases in the PVDF_V and PVDF_ZnO/V_CH nanocomposite films were confirmed. Moderately hydrophilic PVDF nanocomposite films with water contact angle values (WCA) in the range of 58°–69° showed surface stability with respect to the Zeta potential values. The effect of positive or negative Zeta-potential values of nanofillers (ζn) on the resulting negative Zeta-potential values (ζ) of PVDF nanocomposite films was demonstrated. Interaction of PVDF chains with hydroxy groups of vermiculite and amino and imino groups of CH caused transformation of γ-phase to α. The friction properties were evaluated based on the wear testing and mechanical properties were evaluated from the tensile tests based on Young’s modulus (E) and tensile strength (Rm) values. Used nanofillers caused decreasing of friction and mechanical properties of PVDF nanocomposite material films.
24
A critical analysis of the α, β and γ phases in poly(vinylidene fluoride) using FTIR
Xiaomei Cai, Tingping Lei, Daoheng Sun et al. · RSC Advances · 2017 · 1.7K citations · Full text
Natural Sciences, Materials Engineering, Materials Science +14
Vibrational spectrum of PVDF and its interpretation
Ye. Bormashenko, Roman Pogreb, Oleg Stanevsky et al. · Polymer Testing · 2004 · 472 citations
Natural Sciences, Materials Engineering, Materials Science +12
Studies on the transformation process of PVDF from α to β phase by stretching
Li Li, Mingqiu Zhang, Min Zhi Rong et al. · RSC Advances · 2013 · 420 citations
Natural Sciences, Materials Engineering, Materials Science +17