Optik · 2022 · 16 citations · 38 references
EngineeringMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsSurface EngineeringThin FilmsCladding MaterialsCoating ProcessesCoating TechnologyCoatingsLaser Material ProcessingSurface CoatingsFormingLaser CladdingLaser Surface Cladding
A Stellite 6/WC composite coating was prepared on a 60Si2Mn substrate using the method of combing laser cladding and laser re-melting. The effect of different re-melting powers (1400 W, 1500 W and 1600 W) and re-melting scanning speeds (300 mm/min, 500 mm/min and 700 mm/min) on the geometry, microstructure, microhardness and wear resistance of the Stellite 6/WC composite coating was investigated. The research results show that the laser re-melting process can improve the forming quality of the coating and reduce defects such as pores and cracks, but any excessive re-melting power and scanning speed may result in the reoccurrence of defects. With the increase in the re-melting scanning speed, the composite coating shows the evidence of grain refinement. The re-melting power has no significant effect on the microhardness of the coating. When the re-melting scanning speed is 700 mm/min, the microhardness and wear resistance of the corresponding composite coating are the best among all coatings.
38
The redistribution of solute atoms during the solidification of metals
William A. Tiller, Kenneth A. Jackson, J. W. Rutter et al. · Acta Metallurgica · 1953 · 1.7K citations