Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials CharacterizationCeramic RestorationsCrown MaterialsDental CeramicsMaterial DeteriorationOptical CeramicsStructural CeramicsCeramic Material PropertiesColor CoordinatesLithium Disilicate CrownsLoad ResistanceOptical PropertiesThermomechanical Behavior Of CeramicsThermomechanical PropertiesTranslucency Parameter
The aim of this study was to compare the load-to-failure resistance and optical properties of nano-lithium disilicate (NLD) with lithium disilicate (LDS) and zirconia-reinforced lithium silicate (ZLS) in different aging processes. Thirty crowns were milled from NLD, LDS, and ZLS (n = 10). All crowns were subjected to thermomechanical aging and loaded until catastrophic failure. Ten specimens from each material were prepared in two different thicknesses (0.7 mm and 1.5 mm, n = 5), and color coordinates were measured before and after coffee thermocycling. Color differences (ΔE00) and relative translucency parameter (RTP) were calculated. Data were analyzed by using ANOVA and Bonferroni-corrected t-tests (α = 0.05). ZLS had the highest load-to-failure resistance (p ≤ 0.002), while the difference between LDS and NLD was nonsignificant (p = 0.776). The interaction between material type and thickness affected ΔE00 (p < 0.001). Among the 0.7 mm thick specimens, ZLS had the lowest ΔE00 (p < 0.001). Furthermore, 1.5 mm thick ZLS had lower ΔE00 than that of 1.5 mm thick LDS (p = 0.036). Other than ZLS (p = 0.078), 0.7 mm thick specimens had higher ΔE00 (p < 0.001). The interaction between material type, thickness, and thermocycling affected RTP (p < 0.001). Thinner specimens presented higher RTP (p < 0.001). NLD and LDS had higher RTP than ZLS (p ≤ 0.036). However, 0.7 mm thick specimens had similar RTP after coffee thermocycling (p ≥ 0.265). Coffee thermocycling reduced the RTP values of 0.7 mm thick NLD (p = 0.032) and LDS (p = 0.008). NLD may endure the occlusal forces present in the posterior region. However, long-term coffee consumption may impair the esthetics of restorations particularly when thin NLD is used.
39
Translucency thresholds for dental materials
Marianne Salas, Cristina Lucena, Luis Javier Herrera et al. · Dental Materials · 2018 · 281 citations
Dentistry, Dental Biomaterials Science, Dental Materials Science +8