Journal of Polymer Science Part A-1 Polymer Chemistry · 1966 · 46 citations · 5 references
Natural SciencesChemistryMaterials ScienceOrganic ChemistryPolymer ChemistryPolymer MaterialsPolymer StabilityPolymerization ChemistrySolution PolymerizationSynthetic PolymersThermal StabilityThermal Stability Of PolymersThermal StabilizationThermally Stable Polymers
Abstract Six thermally stable polyquinoxalines have been prepared by the reactions of combinations of three tetraamines, 3,3′,4,4′‐tetraaminodiphenyl sulfone (II), and 3,3′,4,4′‐tetraaminodiphenyl ether (V), with two bisglyoxals, 4,4′‐diglyoxalyldiphenyl sulfide dihydrate (III) and 4,4′‐diglyoxalyldiphenyl sulfone dihydrate (IV). The polymers were prepared from polymerization in two stages. The first stage, a solution polymerization, produces an initially low or moderate molecular weight material, which is advanced to a high molecular weight (η inh > 1.0) by heating at 375°C. under reduced pressure. All the polyquinoxalines have excellent thermal stability both in nitrogen and in air and improved solubility.
5
J. K. Stille, J. R. Williamson · Journal of Polymer Science Part B Polymer Letters · 1964 · 52 citations
J. K. Stille, J. R. Williamson · Journal of Polymer Science Part A General Papers · 1964 · 24 citations