IEEE Transactions on Magnetics · 2014 · 18 citations · 18 references
Natural SciencesMaterials EngineeringMaterials ScienceCondensed Matter PhysicsCrystal StructureMagnetic MaterialsFerrimagnetic MaterialsMagnetic CharacterizationMagnetic OxidesMagnetic Properties Of SolidsMagnetism In SolidsX-ray DiffractionDiffraction PatternsFerritesMagnetic Flux DensityMagnetic Materials CharacterizationMagnetic PropertiesMagnetic SaturationSpinel FerritesSpinel Structure
The microstructure and magnetic properties, especially the dc-bias-superposition characteristic of the SnO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> -doped and low-temperature-fired NiCuZn ferrites, were investigated. X-ray diffraction patterns displayed a single-phase spinel structure for all samples. In addition, with the increase of SnO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> content, the average grain size, sintered density, and saturation magnetic flux density (B <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">s</sub> ) gradually decreased. Initial permeability and Q-factor value first increased slightly, and then decreased continuously with further increasing SnO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> content. Under relatively low superposition magnetic field (H <; 140 A/m), a higher initial permeability favored to obtain a higher incremental permeability. However, when the superposition magnetic field continued to increase, some samples with a lower initial permeability displayed a higher incremental permeability. The incremental permeability was mainly determined by B <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">s</sub> , especially coercivity (H <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">c</sub> ) of the samples. The sample with 0.75 wt% SnO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> favored to obtain a better DC-bias-superposition characteristic on incremental permeability and H <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">70%</sub> (the value of the superposition magnetic field when the incremental permeability reduced to 70% of the initial value). Possible mechanisms contributing to the above results were discussed in detail.
18