British Polymer Journal · 1971 · 13 citations · 4 references
Natural SciencesChemistryMaterials ScienceChemical KineticsPolymer ChemistryPolymer EngineeringDegradation ProductsPolymer CharacterizationPolymer DegradationPolymer StabilityPolymer Thin FilmsPolymerization KineticsChemical Degradation KineticsOxidative Degradation AnalysisOxidative Degradation ProductsOxidative Degradation StudiesPolyimidesPolymer Degradation AnalysisPolymer Degradation KineticsPolymer Degradation Mechanisms
Abstract The amounts of unchanged pyromellitimide and diphenylether components in a poly‐N,N′‐(4,4′‐diphenyl‐ether)pyromellitimide film were determined as a function of the time of oxidation at 400°C. Coupling of the diphenylether portion of the chain to give complex aromatic structures occurred at a faster rate than destruction of the pyromellitimide ring. Both these processes were much faster than the overall rate of oxidation as measured by weight loss.
4