Journal of the Japan Society of Powder and Powder Metallurgy · 2000 · 11 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsStructural MaterialsAlloysFerrous MetallurgyInjection MoldingMetalsSinteringStrength Of MaterialsHigh-temperature StrengthInjection Molding TechniqueMechanical Properties Of Sintered MaterialsMetal Injection MoldingTensile DeformationTensile StrainTensile Strength
The B2 FeAl (Fe-40Al and Fe-48Al (at.%)) sintered compacts were prepared by metal injection molding (MIM) process. Then, tensile tests were performed in air at room temperature, 400°C, 600°C and 800°C. The results obtained were summarized as follows.(1) The Fe-48Al compact had the good 0.2% proof stress and tensile strength more than 600 MPa at room temperature. However, they rapidly decreased with increasing test temperature. On the other hand, the 0.2% proof stress of Fe-40Al compact at 400°C and 600°C were almost equal to that at room temperature (-300 MPa). The tensile strength of this compact showed the maximum (680MPa) at 400°C. The tensile strength of both compacts went down to less than 100 MPa at 800°C.(2) At room temperature, the Fe-40Al compact showed the substantial elongation of 2.3%, while that of Fe-48Al compact was only 0.3 %. The elongation of both compacts at 600°C showed high value of 25-30 %. Both compacts changed the fracture mode from brittle to ductile at the temperature range from 400°C to 600°C.