Journal of Applied Physics · 1961 · 146 citations · 3 references
EngineeringMaterials EngineeringMaterials ScienceFormation EvaluationMechanical Behavior Of MaterialsStructural MaterialsFracture CharacterizationFracture MechanicsFracture PropagationBrittle FailureFracture BehaviorFracture Of GlassesFragment Size AnalysisFragment Size DistributionMaterial Fracture BehaviorParticle-size DistributionSieve Analysis
Experimental verification of Gilvarry’s predicted fragment size distribution was achieved by compressively fracturing spherical glass specimens. A gelatin matrix was used to contain fragments and suppress secondary fracture, approximating ideal single‑fracture conditions. Sieve‑analysis data revealed a linear relationship between fracture probability and mean particle size over broad ranges, disproved a log‑normal distribution, showed three peaks instead of two, but full agreement with theory was restored by excluding fragments with original surface, confirming the model down to 1 µm and allowing estimation of internal flaw densities.
The theoretical results of Gilvarry for the size distribution of the fragments in single fracture have been verified experimentally by fracturing spherical glass specimens under compression. The fragments were contained by a gelatin matrix to inhibit secondary fracture and thus make conditions conform as closely as possible to single fracture. Experimental values of the probability of fracture as obtained by sieve analysis show the predicted linear variation with the mean dimension x of the particles, over reasonably large intermediate ranges of the variables. It is shown that a logarithmic-normal distribution does not represent the experimental results. The over-all data exhibit three local maxima in the differential probability of fracture as a function of x, whereas the theory permits only two. Agreement in the number of peaks is obtained by subtracting the contribution to the over-all probability of those fragments containing original surface of the specimen, which yields the true probability considered in the theory. In this manner, reasonably complete agreement between theory and experiment for single fracture is obtained. For plural fracture (carried out without use of gelatin), two additional peaks exist in the curve of the over-all differential probability vs x, as compared to the case for single fracture. The theory of Gilvarry is confirmed down to a fragment dimension of at least 1 μ by means of an electrical counting instrument, and checked by direct microscopic sizing to 5 μ. The results yield numerical values of internal flaw densities, and thus provide a tool to study the distribution of Griffith flaws existing internally in a solid.
3
F. O. Anderegg · Industrial & Engineering Chemistry · 1939 · 88 citations