Enhancing the performance of natural rubber latex with polymeric isocyanate as cold-pressing and formaldehyde free adhesive for plywood

Muhammad Adly Rahandi Lubis, Faizatul Falah, Dian Harini, Sudarmanto, Anggi Kharisma, Budi Tjahyono, Widya Fatrıasarı, Bambang Subiyanto, Lisman Suryanegara, Apri Heri Iswanto

The Journal of Adhesion · 2021 · 16 citations · 26 references

Concepts

Abstract

A cold-pressing and formaldehyde free adhesive for plywood has been prepared by incorporating natural rubber latex (NRL) and poly(vinyl alcohol) (PVA) at a ratio of 1:1 (w/w) with different contents of polymeric 4,4-diphenyl methane diisocyanate (pMDI) (i.e., 0, 1, 3, and 5% based on NRL-PVA solids content). Plywood panel has been manufactured with a glue spread of 200 g/cm2 under a cold-pressing of 5.0 MPa at temperature of 27 ± 2°C for 24 hr. The optimum level of pMDI in NRL-based adhesive is then used to prepare plywood for different pressing times (2, 6, and 12 hr). The result shows that addition of pMDI-created urethane linkages from the reaction between pMDI and NRL-PVA. Increasing pMDI content shortens the gel time of NRL-based adhesive, lowers its curing temperature and activation energy, and increased the solids content and viscosity. Adhesion performance of plywood bonded with NRL-PVA/pMDI adhesive was enhanced and formaldehyde emission was reduced with increasing in pMDI content. Statistical analysis suggested that NRL-PVA/3%pMDI adhesive can be used to manufacture plywood under cold-pressing of 5.0 MPa at temperature of 27 ± 2°C for 12 hr with a dry tensile shear strength of .87 MPa and .09 mg/L of formaldehyde emission.

References

26