Surface Review and Letters · 2021 · 73 citations · 28 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallic MaterialsMetallurgyCoating TechnologyCoatingsLaser Material ProcessingLaser Surface ProcessingMetalsWear-resistant MaterialsHard CoatingsLaser Surface MeltingLaser Surface ModificationMetallic CoatingsMetallurgical Properties In FabricationSurface MeltingWearWear Rates
In this study, NiCrC and NiCrSi coatings are deposited on the MDN 310 steel using High-Velocity Oxy-Fuel (HVOF) process. Laser Surface Melting (LSM) post-heat treatment is carried out on as-sprayed coatings using Laser Engineered Net Shaping (LENS TM ) with a power of 300[Formula: see text]W. The characteristics of both coatings in terms of mechanical and metallurgical properties have been investigated. The thicknesses of the as-sprayed NiCrC and NiCrSi coatings are in the range of 170–200[Formula: see text][Formula: see text]m. Laser-treated NiCrC and NiCrSi coatings exhibit a thickness range of 162–185[Formula: see text][Formula: see text]m, respectively. The microstructure of laser-treated NiCrC-300W coating clearly shows a dendrite-like structure, whereas the laser-treated NiCrSi coating exhibits hard layer and columnar homogeneity. Microhardness of as-sprayed NiCrC coating is [Formula: see text] [Formula: see text] and that of NiCrSi coating is [Formula: see text] HV[Formula: see text]. Microhardness of laser-treated NiCrC coating is [Formula: see text] HV[Formula: see text] and that of NiCrSi coating is [Formula: see text] HV[Formula: see text]. Dry sliding wear tests are conducted at room temperature (RT) and 400 ∘ C with 10-N and 20-N loads. The wear rates at 400 ∘ C temperature of laser-treated NiCrC and NiCrSi coatings produced are slightly below [Formula: see text][Formula: see text]mm 3 /m and [Formula: see text][Formula: see text]mm 3 /m, respectively. Laser-treated coatings produced better dry sliding wear behavior compared with as-sprayed coatings owing to dense microstructure. Formation of SiC phase in NiCrSi coating imparts high wear and frictional resistance compared to the NiCrC coating.
28
Fuat Kara, Mustafa Karabatak, Mustafa Ayyıldız et al. · Journal of Materials Research and Technology · 2019 · 169 citations · Full text
Wear behaviour of laser clad NiCrBSi coating
E. Fernández, M. Cadenas, R. González et al. · Wear · 2005 · 166 citations · Full text
Solid particle erosion of HVOF sprayed WC-Co/NiCrFeSiB coatings
Satya Prakash, S. K. Nath, Pawan Kumar Sapra et al. · Wear · 2010 · 163 citations
Hazoor Singh Sidhu, Buta Singh Sidhu, Satya Prakash · Journal of Materials Processing Technology · 2005 · 117 citations
Natural Sciences, Materials Engineering, Materials Science +17