DentistryMaterials EngineeringMaterials ScienceCeramicsDental MaterialsProsthodontic MaterialsAll-ceramic RestorationsCeramic RestorationsDental CeramicsDenture ProcessingFracture ToughnessCeramic Core RestorationsCrystallizationCrystallization EffectsCrystallization PathwaysFracture Resistance Of RestorationsMonolithic Ceramic RestorationsRandomizationRestorations
The aim of this study was to determine the resistance to fracture of feldspathic restorations with lithium disilicate and crystallized with different ovens and programs. METHODS: Sixty monolithic restorations (LD) (EMAX CAD™ LT, Ivoclar-Vivadent™) were designed with the same parameters and milled with a CAD/CAM system (CEREC SW 5.1, CEREC MCXL, Dentsply-Sirona™, Bensheim). Each restoration was randomly assigned by randomization software (RANDNUM) to one of the three groups: (a) (NF) Oven P310 (Ivoclar, Vivadent) normal crystallization program, (b) (FF) Ivoclar P310 oven (Ivoclar-Vivadent™) rapid crystallization program, or (c) (SF) SpeedFire oven (Dentsply-Sirona™). RESULTS: < 0.05). The NF and FF groups showed the highest values of resistance to fracture, with statistically significant differences with the SF group. CONCLUSIONS: Using a furnace from the same dental company with predetermined programs from the material manufacturer, as well as using a predetermined program for rapid crystallization, has no effect on fracture resistance, and would save clinical time when performing ceramic restorations with lithium disilicate, while keeping their mechanical properties.
24
The evolution of the CEREC system
Werner Mörmann · The Journal of the American Dental Association · 2006 · 389 citations · Full text
Arthur Furtado de Mendonça, Mahdi Shahmoradi, Cresus Vinícius Depes de Gouvêa et al. · Journal of Prosthodontics · 2018 · 170 citations
Dentistry, Dental Materials Science, Restorative Dentistry +17