Vitrimer Transition Temperature Identification: Coupling Various Thermomechanical Methodologies

Amber M. Hubbard, Yixin Ren, Dominik Konkolewicz, Alireza S. Sarvestani, Catalin R. Picu, Gary S. Kedziora, Ajit K. Roy, Vikas Varshney, Dhriti Nepal

ACS Applied Polymer Materials · 2021 · 118 citations · 43 references

Concepts

TL;DR

Vitrimers promise adaptive shape reconfigurability, welding, and self‑healing through dynamic covalent reactions above the vitrimer transition temperature (Tv), yet reported Tv values vary with chemistry and measurement methods, making precise understanding essential for designing recyclable actuators and structural adhesives. The study introduces data‑interpretation techniques for stress‑relaxation and elongational creep that reconcile multiple Tv measurement methods and demonstrates that heating rate, axial force, and catalyst concentration critically determine the Tv range. These techniques are coupled with a kinetic model of the transesterification rate‑limiting step, which captures the temperature dependence and aligns closely with experimental data. The results show that altering catalyst concentration or heating rate can shift Tv by up to 115 °C and 43 °C, respectively, confirming the pivotal role of experimental parameters and validating the kinetic model.

Abstract

Vitrimers hold great promise as adaptive materials capable of shape reconfigurability, welding, and self-healing due to dynamic covalent reactions occurring above the vitrimer transition temperature (Tv). Previous literature reports the Tv as one value influenced mainly by chemistry; however, literature also reports significant inconsistencies when measuring or identifying Tv trends. Herein, we present unique data interpretation methods to analyze stress–relaxation and elongational creep results allowing for excellent agreement between multiple Tv measurement methodologies. We also demonstrate that experimental parameters (e.g., heating rate and applied axial force) and catalyst concentration are crucial in dictating the Tv range. Varying the catalyst concentration or sample heating rate shifts the Tv up to 115 and 43 °C, respectively. Additionally, we present a kinetic model confirming the temperature dependence of the transesterification rate-limiting step, exhibiting excellent agreement with experimental data. Fundamentally understanding the Tv will inform future design of vitrimers toward applications ranging from recyclable actuators to structural adhesives.

References

43