Metals · 2020 · 23 citations · 33 references
Natural SciencesMaterials EngineeringMaterials ScienceMetallurgyPhase TransformationsSolidificationAlloy SolidificationAlloysCastingKinetics Of Phase TransformationsMetalsMicrostructure EvolutionAgeingAlloy Solidification MicrostructureDuctility EnhancementDuctility LossFormingHomogenizationHot FormingSilicon-containing Alloys
In the as-cast state, Al–Mg–Si alloys are not suitable for hot forming. They present low ductility due to the presence of intermetallic β-AlFeSi particles that form in the interdendritic regions during the solidification process. Homogenization treatments promote the transformation of these particles into α-(FeMn)Si particles, which are smaller in size and more rounded in shape, thus improving the ductility of the material. This paper analyses the influence of various solution treatments on the transformation of β-AlFeSi particles into α-(FeMn)Si particles in an Al 6063 alloy. Their effect on different ageing treatments in the 150–180 °C temperature range is also studied. An increase in the solution temperature favours greater transformation of the β-AlFeSi particles into α-(FeMn)Si, dissolving a greater amount of Si, thereby having a significant effect on subsequent ageing. We found that as the dwell time at a temperature of 600 °C increases, the rate of dissolution of the Fe atoms from α-(FeMn)Si particles exceeds the rate of incorporation of Mn atoms into said particles. This seems to produce a delay in reaching the peak hardness values in ageing treatments, which warrants further research to model this behaviour. The optimal solution treatment takes place at around 600 °C and the highest obtained peak hardness value is 104 HV after a 2 h solution treatment at said temperature and ageing at 160 °C for 12 h.
33
The precipitation sequence in Al–Mg–Si alloys
Geoffrey A. Edwards, Krystyna Stiller, G. L. Dunlop et al. · Acta Materialia · 1998 · 1.4K citations
Natural Sciences, Materials Engineering, Materials Science +11