Publication | Closed Access
Clinical Evaluation of Chairside-Fabricated Partial Crowns Made of Zirconia- Reinforced Lithium Silicate Ceramic - 2-Year-Results.
11
Citations
0
References
2020
Year
To avoid early material-related fractures, observing the recommended minimum thickness of 1.0 mm is essential. However, further validation of these results in studies with longer observational periods is required.