Materials · 2020 · 20 citations · 38 references
Natural SciencesChemical EngineeringMaterials ScienceCatalysisInorganic ChemistrySurface ScienceCatalyst PreparationCatalyst StabilityCatalytic MaterialsAgeingAgeing EffectsAging MechanismsHydrothermal TreatmentPore VolumePore Volume CharacterizationSpecific Surface AreaTemperature Effects On Decomposition
Cu-ZSM-5 and Ce-doped Cu-Ce-ZSM-5 samples were prepared by liquid-phase ion exchange method. The two catalysts were subjected to hydrothermal aging treatment in the simulated flue gas of a coal-fired power station at an ageing temperature of 650–850 °C. The denitration experiment found that the activity of the aged Cu-ZSM-5 was 19.6% to 41% lower than that of the fresh Cu-ZSM-5 at the optimal decomposition temperature of NO at 550 °C, while the aged Cu-Ce-ZSM-5 had only a 14.8% to 31.5% reduction in activity than the fresh Cu-Ce-ZSM-5. The samples were characterized by XRD, BET, H2-TPR, XPS, NO-TPD, etc. The results showed that hydrothermal aging treatment leads to the dealumination of the ZSM-5 framework and reduces the specific surface area and pore volume of the micropore in the sample. It also exacerbates the isolated Cu2+, and the active center {Cu2+-O2−-Cu2+}2+ dimers migrate towards the sample surface and form inactive CuO. Doping with Ce can promote the dispersion of Cu(OH)+, which was the precursor of {Cu2+-O2−-Cu2+}2+. Ce3+ can preferentially occupy the less active bridged hydroxyl exchange sites, so that copper ions occupy the more active aluminum hydroxyl sites, thereby inhibiting the migration of active centers.
38
Effects of hydrothermal aging on NH3-SCR reaction over Cu/zeolites
Ja Hun Kwak, Diana Tran, Sarah Burton et al. · Journal of Catalysis · 2012 · 520 citations
Junjie Xue, Xinquan Wang, Gongshin Qi et al. · Journal of Catalysis · 2012 · 401 citations