Journal of the American Ceramic Society · 2019 · 22 citations · 23 references
DentistryMaterials EngineeringMaterials ScienceCeramicsMechanical Behavior Of MaterialsMechanical Properties Of Dental MaterialsFracture MechanicsFracture ResistanceFracture ToughnessGlass MaterialsIndentation PropertiesStress-strain BehaviorDensificationFracture Of GlassesGlass Fracture BehaviorGlass Fracture ToughnessIndentation Fracture ToughnessIndentation StrengthMechanical Properties Of GlassesToughness Of Glasses
Abstract The fracture toughness was measured by the Vickers indentation method and by chevron notch for a series of x CaO‐ x Al 2 O 3 ‐(100 − 2 x )SiO 2 glasses. As the silica content was increased, the fixed ξ value Vickers indentation fracture toughness (IFT) values increased, while the chevron notch values decreased. Glasses with higher silica contents deform with more densification and less shear when indented with a Vickers tip, thus resulting in reduced residual stress in the region surrounding the indent. The reduction in residual stress for high silica glasses results in less median/radial crack extension and unreasonably high Vickers IFT values. This indicates that a fixed ξ value of 0.016 is not appropriate for the glasses in this series. By repeating the IFT method with a sharper 110° four‐sided pyramidal diamond indenter, it is demonstrated that indentation toughness and chevron notch toughness values now trend in the same direction and are in good agreement with a fixed ξ value of 0.0297. With the sharper indenter tip, the densification component to the deformation is substantially reduced for all glass types such that it no longer has such a prominent influence on the residual stress field. This result suggests that a fixed ξ value IFT method may be appropriate for all glass types if a sharper indenter tip is substituted in the place of the Vickers tip.
23