Improved Properties of Doped BaTiO<sub>3</sub> Piezoelectric Ceramics

Rémy Ul, Pascal Marchet, Maï Pham-Thi, Louis-Pascal Tran-Huu-Hue

physica status solidi (a) · 2019 · 23 citations · 32 references

Concepts

Abstract

(Ca z Ba 1 − z )(Ti 1 − x − w Co x Nb w )O 3 − δ lead‐free piezoelectric ceramics are prepared using solid‐state reactions. The use of a Li 2 O sintering aid enables one to obtain dense ceramics at a temperature of 1100 °C instead of the 1350 °C used for BaTiO 3 (BT) in conventional sintering. X‐ray diffraction (XRD) data indicate structural modifications, suggesting insertion of the doping elements into the tetragonal structure. The insertion of Li/Ca/Co/Nb improves piezoelectric properties: for micrograin‐size ceramics, a piezoelectric charge constant and an electromechanical coupling factor of d 33 = 255 pC N −1 and k p = 43.5% are reached, respectively. Furthermore, a thermal annealing of the cobalt‐doped sample at 1080 °C under O 2 atmosphere leads to d 33 = 280 pC N −1 and k p = 44.6%. BaTiO 3 :Co ceramics present distorted ferroelectric cycles due to the occurrence of an internal bias field. The high mechanical quality factors ( Q m &gt; 1000) obtained for the doped BT ceramics afford stability against electrical stress of up to 500 V RMS mm −1 , which makes these materials competitive with PZT4 for some applications.

References

32