Rare Metals · 2019 · 22 citations · 26 references
Natural SciencesMaterials SciencePhysicsCeramic MaterialsCeramicsMagnetic MaterialsFerrimagnetic MaterialsMagnetic CeramicsMagnetic CharacterizationMagnetic OxidesMagnetic Properties Of SolidsMagnetic SusceptibilityAnisotropy In FerritesFerrimagnetic OxidesFerritesMagnetic Materials CharacterizationMagnetic PropertiesStrontium SaltsThermomagnetic Properties
Abstract The effects of heat treatment conditions on the magnetic properties and microstructure of M‐type strontium ferrite according to calcination temperature were analyzed. Strontium ferrite Sr 0.06 Ca 0.52 La 0.52 Fe 11.68 Co 0.22 O 19 magnetic powder was prepared by a standard ceramic process. During experiments, the calcination temperature was varied from 1180 to 1260 °C, and sintering temperature was fixed. While the M‐phase (SrFe 12 O 19 ) existed with hematite (Fe 2 O 3 ) in the powder calcined at below 1220 °C, the pure M‐phase was observed in the powder calcined at over 1240 °C. With an increase in the calcination temperature, the magnetization of the calcined powder increases, meanwhile, the coercivity decreases. The magnetization is improved by decreasing the lattice constant c and activating the Fe 3+ –O–Fe 3+ superexchange interaction, and the coercivity decreases by the large particle sizes due to the grain growth.
26