Applied Sciences · 2019 · 14 citations · 19 references
EngineeringMaterials EngineeringMaterials ScienceManufacturing ProcessesMaterials ProcessingMechanical Behavior Of MaterialsFabrication MaterialsInjection MoldingMetal FabricationPowder ProcessingPowder TechnologySinteringBinder SystemsMetal Injection MoldingPowder Feedstock PreparationPrecision Injection MoldingTensile StrengthUltimate Tensile StrengthViscosityYield Strength
In this study, the metal injection molding (MIM) process is applied to produce Ti-6Al-4V parts using blended and prealloyed powders, respectively. The feedstocks are prepared from a polyformaldehyde-based binder system with a powder loading of 60 vol%, exhibiting a low viscosity. The decomposition behavior of the binders is investigated and the thermal debinding procedure is designed accordingly. The debound parts are subsequently sintered at 1200 and 1300 °C. The results show the mechanical properties of the sintered samples prepared from blended powder are comparable to those prepared from prealloyed powder, with yield strength of 810 MPa, ultimate tensile strength (UTS) of 927 MPa, and elongation of 4.6%. The density of the as-sintered samples can reach 4.26 g/cm3 while oxygen content is ~0.3%. Based on the results, watch cases with complex shapes are successfully produced from Ti-6Al-4V blended powder. The case gives a good example of applying metal injection molding to mass production of precise Ti-6Al-4V parts with complex shapes in a cost-effective way.
19
Review of the Methods for Production of Spherical Ti and Ti Alloy Powder
Pei Sun, Zhigang Zak Fang, Ying Zhang et al. · JOM · 2017 · 263 citations · Full text