Operative Dentistry · 2018 · 26 citations · 23 references
Dentin NTAP treatment for 30 seconds contributed to higher μTBS after two years of water storage in the ER approach, while no difference was observed among treatments in the SE evaluation. This result might be correlated to the increase in nanohardness and Young's modulus of the hybrid layer and to better adhesive infiltration, since dentin hydrophilicity was also improved. Although some effects were observed using NTAP for 10 seconds, the results suggest that 30 seconds is the most indicated treatment time.
23
W. C. Oliver, George M. Pharr · Journal of materials research/Pratt's guide to venture capital sources · 1992 · 26.1K citations
Comparative Study on Adhesive Performance of Functional Monomers