Efficient laser operations of unprocessed thin plate of Nd:YPO<sub>4</sub> crystal

Xuzhao Zhang, Jie He, Tianhong Tang, Bing Teng, Degao Zhong, Xinguang Xu, Zhengping Wang

Optics Express · 2018 · 23 citations · 27 references

DOIFull text

Open access

Concepts

Abstract

, 156 μs, respectively. With an as-grown 0.6 mm thin slice which was unpolished and uncoated, efficient diode-pumped continue-wave (CW) laser operations were realized at 1.06 and 1.3 μm wavebands. The 1063 nm output power reached 2.16 W when the absorbed pump power was 4.07 W, corresponding to an optical-to-optical efficiency of 53%, and a slope efficiency of 56.4%. The 1.3 μm laser output exhibited the simultaneous operations of dual-wavelengths, i.e. 1338 and 1347 nm. The maximum output power was 800 mW at an absorbed pump power of 3.08 W, giving an optical-to-optical efficiency of 26% and a slope efficiency of 28.2%.