Investigation and modelling of work roll temperature in induction heating by finite element method

Li Bao, Xiwei Qi, R-B. Mei, Xinyu Zhang, GL Li

Journal of the Southern African Institute of Mining and Metallurgy · 2018 · 15 citations · 10 references

DOIFull text

Open access

Concepts

Abstract

Hot and warm rolling technology has been used widely to produce various metal strip products since 1880, when Japan first began steel production In hot rolling, the workpiece is usually heated in a furnace and the temperature decreases significantly during the subsequent slab or strip rolling process. The decreased surface temperature may cause non-uniform deformation and crack generation, especially in metals with poor plastic deformability, such as magnesium and high-silicon steel. The advantage of rolling mills with heated equipment compared to conventional rolling mills was also discussed in detail. Cr 3 C 2 was used as the roll sleeve and steel as the main body of the work roll (Fischer and Yi, 1964). After that, methods and equipment for rolling with a heated work roll were proposed and designed by different researchers (Kang, Wang, and Lv 2005; Zhang, Wang, and Wang, 2008; Li et al., 2012) in order to avoid surface oxidation and improve the plastic deformation limit of hardto-form materials. The preheated work roll is significantly helpful for large plastic deformation and grain refinement. Jeong and Ha (2007) discussed the influence of the work roll temperature, initial thickness, thickness reduction, rolling temperature, and rolling velocity on the microstructure and texture of AZ31 magnesium alloy during warm rolling. No cracks were found in the strip with a reduction of 30%, rolling velocity of 30 m/min, rolling temperature of 200C, and work roll temperature of 110C. Furthermore, the grain size was refined significantly with a singlepass 50% reduction after preheating of the work roll. Kim et al. (2014) used a preheated work roll to realize continuous high-ratio differential speed rolling, maintaining the strip temperature within an ideal range for large plastic deformation and dynamic recrystallization. This method refined the grain size of the workpiece from 11.1 m to 2.3 m.

References

10