International Journal of Cast Metals Research · 2018 · 19 citations · 17 references
EngineeringMaterials EngineeringMaterials ScienceMaterials ProcessingMetallic MaterialsMetallurgyAlloy SolidificationAlloysGrain RefinementGrain Structure FormationMetalsSolidification Of MetalsAlloy Composition EffectsAluminium AlloysAluminum AlloysAluminum MetallurgyAluminum-containing AlloysGrain RefinersGrain Structure ControlRefining
The present study was carried out on ultra-pure aluminum, 1050, and 356 alloys. The results revealed that when Al-4%B is added to ultra-pure aluminum, it forms AlB12 and AlB2 which have no grain refining effect in pure aluminum. When no grain refiner is added to pure aluminum, the microstructure is a mixture of columnar and equiaxed grains. The addition of 30 ppm Ti to pure aluminum is sufficient to promote equiaxed grains when the metal is solidified at high rate ~ 10°C/s but requires an addition of 1000 ppm B at 0.8°C. Increasing the Si content to 7% reduces the initial grain size of pure aluminum from 2800 μm to 1200 μm. In commercial aluminum, B reacts with traces of Ti to form TiB2 phases which are active grain refining agents. However, in Al-7%Si, Ti reacts with Si forming (Al,Si)2Ti phase which is a poor refining agent.
17