ACS Energy Letters · 2018 · 268 citations · 46 references
Natural SciencesChemistryMaterials ScienceCatalysisSurface ChemistrySurface ScienceMetal Oxide NanomaterialsMetal OxidesSurface CatalysisSurface Chemistry Of SolidsSurface OxidationSurface ReactionsCatalyst ActivityCatalytic ActivityDissolution StabilityMetal Oxide Oxygen Evolution CatalystsNanoparticlesOxygen Evolution ReactionRutile OxidesTransition Metal Oxides
Rutile RuO2 catalysts are the most active pure metal oxides for oxygen evolution; however, they are also unstable toward dissolution. Herein, we study the catalytic activity and stability of oriented thin films of RuO2 with (111), (101), and (001) orientations, in comparison to a (110) single crystal and commercial nanoparticles. These surfaces were all tested in aqueous solutions of 0.05 M H2SO4. The initial catalyst activity ranked as follows: (001) > (101) > (111) ≈ (110). We complemented our activity data with inductively coupled plasma mass spectroscopy, to measure Ru dissolution products occurring in parallel to oxygen evolution. In contrast to earlier reports, we find that, under our experimental conditions, there is no correlation between the activity and stability.
46
Universality in Oxygen Evolution Electrocatalysis on Oxide Surfaces
Isabela C. Man, Hai‐Yan Su, Federico Calle‐Vallejo et al. · ChemCatChem · 2011 · 4.6K citations
Electrolysis of water on oxide surfaces
Jan Rossmeisl, Zheng‐Wang Qu, Hui Zhu et al. · Journal of Electroanalytical Chemistry · 2007 · 3K citations
Serhiy Cherevko, Simon Geiger, Olga Kasian et al. · Catalysis Today · 2015 · 1.4K citations