Physical Chemistry Chemical Physics · 2018 · 39 citations · 32 references
Natural SciencesChemistryMaterials ScienceMaterials ChemistryPhysical ChemistryThin FilmsCrystal GrowthPhysical Vapor DepositionSolid-liquid InterfacesSurface PhysicsThin-film DepositionThin-film MaterialsAngle-resolved Photoelectron SpectroscopyAngle-resolved X-ray Photoelectron SpectroscopyFilm MorphologyGrowth KineticsInitial Film MorphologyIonic LiquidsThin-film Growth KineticsThin-film Morphology
Various amounts of the ionic liquids (ILs) [C1C1Im][Tf2N] and [C8C1Im][Tf2N] were deposited in vacuo by physical vapour deposition (PVD) on single crystalline Ag(111) at room temperature and subsequently monitored by angle-resolved X-ray photoelectron spectroscopy (ARXPS) as a function of time. For very low coverages of up to one closed molecular layer, an initial wetting layer was rapidly formed for both ILs. Deposition of higher amounts of [C1C1Im][Tf2N] revealed an initial three-dimensional film morphology. On the time scale of hours, characteristic changes of the XPS signals were observed. These are interpreted as island spreading and a transformation towards a nearly two dimensional [C1C1Im][Tf2N] film as the final state. In contrast, a film morphology close to 2D was found from the very beginning for [C8C1Im][Tf2N] deposited on Ag(111) demonstrating the influence of the alkyl chain length on the growth kinetics. These studies also highlight the suitability of time-resolved ARXPS for the investigation of IL/solid interfaces, which play a crucial role in IL thin film applications such as in catalysis, sensor, lubrication, and coating technologies.
32
Dzmitry H. Zaitsau, Gennady J. Kabo, Aliaksei A. Strechan et al. · The Journal of Physical Chemistry A · 2006 · 561 citations
Hans‐Peter Steinrück, Peter Wasserscheid · Catalysis Letters · 2014 · 397 citations · Full text