Preparation and characterization of zirconia-alumina system via solution and solid phase mixing method

Yanwar Faza, Zulia Hasratiningsih, Andrie Harmaji, I Made Joni

AIP conference proceedings · 2018 · 11 citations · 12 references

DOIFull text

Open access

Concepts

Abstract

Popularity of zirconia gained up after discovering the unique properties of zirconia called transformation toughening. Alumina is one of material used to stabilize tetragonal crystalline of zirconia in room temperature. In this study, zirconia-alumina systems have been developed in two ways mixing methods through sol-gel technique. First method was done by mixing both precursors of zirconia and alumina in the hydrolysis stage, while the second method was in the drying stage of the sol-gel technique. Phase of material was solution at hydrolisis stage and solid at drying stage. Zirconia-alumina system having the ratio 90:10 by weight (ZrO2:Al2O3). The mixture were calcined at temperature 900 °C for 2 hours. Samples were than characterized by X-Ray Diffraction to assign tetragonal crystallline of zirconia. Scanning Electron Microscope and Brunauer-Emmett-Teller characterization were conducted to observe morphology, particle size as well as surface area of samples. XRD characterization of solution phase mixing sample exhibited 94.5% tetragonal crystalline and 5.5% monoclinic crystalline. The solid phase mixing sample were 25.3% tetragonal crystalline and 74.7% monoclinic crystalline. SEM characterization showed agglomeration for both samples with particle size 8.72 µm for solution mixing method and 11.17 µm for solid mixing method. However, nano size particle were also identified. Surface area of mixed oxide are 14.164 m2/g and 13.996 m2/g respectively. As a conclusion, this results confirmed that solution mixing method was more effective to produce tetragonal crystalline of zirconia than solid phase mixing method.

References

12