The Journal of Advanced Prosthodontics · 2017 · 26 citations · 43 references
DentistryDental Materials ScienceProsthodonticsDental MaterialsMechanical Properties Of Dental MaterialsProsthodontic MaterialsAll-ceramic RestorationsCeramic RestorationsCrown FracturesCrown MaterialsDental CeramicsTooth Preparation DesignAxial Wall ReductionCeramic Crown SystemsDeep Chamfer Finish LineDental CrownsLithium Disilicate CrownsMonolithic Ceramic RestorationsThermo-mechanical LoadingTooth Reduction Depth
PURPOSE: To investigate the effect of reducing tooth preparation and ceramic thickness on fracture resistance of lithium disilicate crowns. MATERIALS AND METHODS: Specimen preparation included a standard complete crown preparation of a typodont mandibular left first molar with an occlusal reduction of 2 mm, proximal/axial wall reduction of 1.5 mm, and 1.0 mm deep chamfer (Group A). Another typodont mandibular first molar was prepared with less tooth reduction: 1 mm occlusal and proximal/axial wall reduction and 0.8 mm chamfer (Group B). Twenty crowns were milled from each preparation corresponding to control group (n=5) and conditioned group of simultaneous thermal and mechanical loading in aqueous environment (n=15). All crowns were then loaded until fracture to determine the fracture load. RESULTS: >.05) in Group A. CONCLUSION: Reducing the amount of tooth preparation by 0.5 mm on the occlusal and proximal/axial wall with a 0.8 mm chamfer significantly reduced fracture load of the restoration. Tooth reduction required for lithium disilicate crowns is a crucial factor for a long-term successful application of this all-ceramic system.
43
Single tooth bite forces in healthy young adults
Virgilio F. Ferrario, Chiarella Sforza, Graziano Serrao et al. · Journal of Oral Rehabilitation · 2004 · 371 citations