Journal of The Electrochemical Society · 2017 · 45 citations · 35 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsMetallurgyCorrosion MechanismsCorrosion Of SteelsCorrosion ResistanceCorrosion-resistant MaterialsPitting CorrosionSteel MaterialsCorrosion Resistance MaterialsLow-carbon SteelMartensitic MicrostructureMartensitic Steel CorrosionMartensitic SteelsMicrostructure Effects On CorrosionPolarization MeasurementsSteel Corrosion Resistance
The pitting corrosion resistance of AISI 1045 carbon steel with as-quenched, tempered, and low-carbon martensitic microstructures was investigated in boric-borate buffer solutions with and without NaCl. Analysis by micro-scale polarization found that tempering and decarburizing treatments decreased the pitting corrosion resistance of as-quenched martensite. The high corrosion resistance of the as-quenched martensite was likely due to the large amount of interstitial carbon. The pitting corrosion resistances of as-quenched martensite, primary ferrite, and pearlite were compared using micro-scale polarization measurements. It was determined that the pitting corrosion resistances of the typical steel structures were ordered as follows: (high) as-quenched martensite > tempered martensite ≈ primary ferrite > pearlite (low). The pitting corrosion resistance of steel was shown to depend on its microstructure.
35
Thermodynamics and phase diagram of the Fe-C system
John Chipman · Metallurgical Transactions · 1972 · 391 citations