Deterioration mechanism of LiNi<sub>0.8</sub>Co<sub>0.15</sub>Al<sub>0.05</sub>O<sub>2</sub>/graphite–SiO<sub>x</sub> power batteries under high temperature and discharge cycling conditions

84

Citations

49

References

2017

Year

Abstract

The capacity degradation of NCA/graphite–SiO<italic>x</italic> batteries under high temperature is attributed to lithium loss from the NCA cathode and structure decay of the graphite–SiO<italic>x</italic> anode.