IEEE Journal of Photovoltaics · 2017 · 33 citations · 5 references
EngineeringMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsSurface EngineeringDurabilityMaterial DurabilityStrength Of MaterialsStructural ReliabilityThin Film AdhesionAdhesion StrengthAdhesion TestingAdhesion WorkAdhesive StrengthBond StrengthDelaminationModule Reliability AnalysisSolar Panel Reliability
The width-tapered cantilever beam method is used to quantify the debond energy (adhesion) of encapsulant and backsheet structures of 32 modules collected from the field. The collected population of modules contains both those that have remained intact and those with instances of either or both encapsulant and backsheet delamination. From this survey, initial threshold values (an adhesion value above which a module should remain intact throughout its lifetime) for encapsulant and backsheet interfaces are proposed. For encapsulants this value is ~160 J/m <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> and for backsheets ~10 J/m <sup xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sup> . It is expected that these values will continue to be refined and evolve as the width-tapered cantilever beam method gets adopted by the PV industry, and that they may aid in the future improvement of accelerated lifetime tests and the development of new, low-cost materials.
5