Journal of Polymer Science Part A Polymer Chemistry · 2017 · 18 citations · 55 references
Natural SciencesChemistryMaterials ScienceOrganic ChemistryPolymer ChemistryPolymer MaterialsGreen Polymer ChemistryPolymer CharacterizationPolymerization ChemistryBio-based Polymer CompoundsLignin ChemistryLignin-derived CompoundsPolyanhydridesPolymers Derived From PhenylpropanoidsResistance To Organic SolventsSolubilityViscosity
ABSTRACT Two new bio‐based diacylhydrazide monomers, namely, 4,4′‐(propane‐1,3‐diylbis(oxy))bis(3‐methoxybenzohydrazide) and 4,4′‐(propane‐1,3‐diylbis(oxy))bis(3,5‐dimethoxybenzohydrazide) were synthesized starting from lignin‐derived phenolic acids, namely, vanillic acid and syringic acid. A series of poly(amide imide)s was synthesized by polycondensation of these diacylhydrazide monomers with commercially available aromatic dianhydrides. Poly(amide imide)s showed inherent viscosity in the range 0.44–0.56 dL g −1 and exhibited good solubility in organic solvents. Poly(amide imide)s could be cast into transparent, flexible, and tough films from their N , N ‐dimethylacetamide solutions. Poly(amide imide)s showed 10% weight loss in the temperature range 340–364 °C indicating their good thermal stability. Glass transition temperature ( T g ) of poly(amide imides)s were measured by DSC and DMA which were in the range 201–223 °C and 214–248 °C, respectively. The T g values of poly(amide imide)s were dependent on the number methoxy substituents on aromatic rings of diacylhydrazide monomers. Molecular dynamics simulation studies revealed that chain rigidity is the dominant factor for observed trends in T g . © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2017 , 55 , 3636–3645
55
Purification of Laboratory Chemicals
Colin Eaborn · Journal of Organometallic Chemistry · 1989 · 4.4K citations