ACS Catalysis · 2017 · 108 citations · 68 references
Natural SciencesChemical EngineeringChemistryCatalysisGreen ChemistryReaction EngineeringCatalytic MaterialsCatalytic MechanismsCatalytic Reaction KineticsFatty Acid ChemistryFatty Acid OxidationFatty Acid SynthesisCatalyst MechanismsCatalyst Structure - Activity RelationshipsCatalytic Reaction MechanismsDehydration ReactionsHydrodeoxygenationLangmuir-hinshelwood MechanismLangmuir-hinshelwood ReactionsRate-determining Step
Highly active bulk transition-metal phosphides (WP, MoP, and Ni 2 P) were synthesized for the catalytic hydrodeoxygenation of palmitic acid, hexadecanol, hexadecanal, and microalgae oil. The specific activities positively correlated with the concentration of exposed metal sites, although the relative rates changed with temperature due to activation energies varying from 57 kJ mol –1 for MoP to 142 kJ mol –1 for WP. The reduction of the fatty acid to the aldehyde occurs through a Langmuir–Hinshelwood mechanism, where the rate-determining step is the addition of the second H to the hydrocarbon. On WP, the conversion of palmitic acid proceeds via R-CH 2 COOH → R-CH 2 CHO → R-CH 2 CH 2 OH → R-CHCH 2 → R-CH 2 CH 3 (hydrodeoxygenation). Decarbonylation of the intermediate aldehyde (R-CH 2 COOH → R-CH 2 CHO → R-CH 3 ) was an important pathway on MoP and Ni 2 P. Conversion via dehydration to a ketene, followed by its decarbonylation, occurred only on Ni 2 P. The rates of alcohol dehydration (R-CH 2 CH 2 OH → R-CHCH 2 ) correlate with the concentrations of Lewis acid sites of the phosphides.
68
Trends in the Exchange Current for Hydrogen Evolution
Jens K. Nørskov, Thomas Bligaard, Á. Logadóttir et al. · Journal of The Electrochemical Society · 2005 · 5.9K citations · Full text
Edward Furimsky · Applied Catalysis A General · 2000 · 1.2K citations