Fabrication, Pressure Testing, and Nanopore Formation of Single-Layer Graphene Membranes

Kumar Varoon Agrawal, Jesse D. Benck, Zhe Yuan, Rahul Prasanna Misra, Ananth Govind Rajan, Yannick Eatmon, Suneet Kale, Ximo S. Chu, Duo O. Li, Chuncheng Gong,

The Journal of Physical Chemistry C · 2017 · 57 citations · 73 references

DOIFull text

Open access

Concepts

TL;DR

Single‑layer graphene membranes promise ultrahigh flux and high selectivity for gas separations, yet it remains unclear whether large‑area membranes can withstand industrial pressure and temperature conditions and how to create controlled molecular‑sized pores. We fabricated low‑defect, free‑standing 5 µm SLG membranes and performed pressure testing, temperature cycling, and gas permeance measurements to evaluate their performance. The membranes exhibited remarkable chemical and mechanical stability—remaining intact over weeks at >0.5 bar, 25–200 °C cycling, and 15 mol % ozone exposure—served as molecularly impermeable barriers, and 1077 °C O₂ etching produced ~1 nm nanopores imaged by STM, demonstrating a viable platform for in‑situ fabrication and testing of graphene gas‑separation membranes.

Abstract

Single-layer graphene (SLG) membranes have great promise as ultrahigh flux, high selectivity membranes for gas mixture separations due to their single atom thickness. It remains a central question whether SLG membranes of a requisite area can exist under an imposed pressure drop and temperatures needed for industrial gas separation. An additional challenge is the development of techniques to perforate or otherwise control the porosity in graphene membranes to impart molecularly sized pores, the size regime predicted to produce high gas separation factors. Herein, we report fabrication, pressure testing, temperature cycling, and gas permeance measurements through free-standing, low defect density SLG membranes. Our measurements demonstrate the remarkable chemical and mechanical stability of these 5 μm diameter suspended SLG membranes, which remain intact over weeks of testing at pressure differentials of >0.5 bar, repeated temperature cycling from 25 to 200 °C, and exposure to 15 mol % ozone for up to 3 min. These membranes act as molecularly impermeable barriers, with very low or near negligible background permeance. We also demonstrate a 1077 °C temperature O2 etching technique to create nanopores on the order of ∼1 nm diameter as imaged by scanning tunneling microscopy, although transport through such pores has not yet been successfully measured. Overall, these results represent an important advancement that will enable graphene gas separation membranes to be fabricated, tested, and modified in situ while maintaining remarkable mechanical and thermal stability.

References

73