The Incidence and Avoidance of Gassing Defects in Chemical and Electropolishing of Aluminium

A. W. Clifford, D. J. Arrowsmith

Transactions of the IMF · 1978 · 10 citations · 2 references

Concepts

Abstract

SummaryThe chemical polishing of aluminium in phosphoric-sulphuric-nitric acid, with and without dissolved copper, has been studied over a wide range of conditions. The number, size and shape of defects caused by gassing have been shown by scanning electron microscopy to depend on potential, electrolyte composition (nitric acid and copper content in particular) and the quality of the aluminium. The gassing defects are shown to have a central mound surrounded by an annular groove and are completely different from etch pits. Practical conditions to avoid gassing defects and pitting in chemical polishing of aluminium are given. The avoidance of gassing defects in electropolishing aluminium is also discussed.