Journal of the Japan Institute of Metals and Materials · 1978 · 23 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsRheologyAluminum OxidesInorganic MaterialsMetal OxidesGlass ViscositySilica-based MaterialsSilicate ChemistrySilicate GlassesViscosity
The results of viscosity measuerments for Na2O-SiO2-Al2O3 and PbO-SiO2-Al2O3 systems and the previous data for CaO-SiO2-Al2O3 and MnO-SiO2-Al2O3 systems have been used to evalute the effect of Al2O3 on the viscosity of the ternary aluminosilicate MO-SiO2-Al2O3 system in the range of molar ratio Al2O3/MO<1. The results obtained are summarized as follows:(1) In the Na2O-SiO2-Al2O3 system, the viscosity greatly increased with the substitution of Al2O3 for SiO2 and the value of SiO2-equivalence of Al2O3 calculated from the resutls was about 1.65. In this system, it was considered that Al-ion forms oxygen tetrahedron likewise Si-ion and acts as the aluminosilicate anion.(2) In the PbO-SiO2-Al2O3 System, the viscosity slightly increased and the rate of increase decreased with decreasing basicity of melts.(3) In the CaO-SiO2-Al2O3 and MnO-SiO2-Al2O3 systems, the viscosity decreased in the range of molar ratio MO/SiO2<1 with increasing concentration of Al2O3 and the rate of decrease became larger with decreasing basicity of melts. Therefore accurate assessment of the results of these systems could not be made simply by the values of SiO2-equivalence of Al2O3.(4) Satisfactory results were obtained by arranging the viscosity data by each alminosilicate using a parameter (nSi+xnAl)⁄nO, the value which corresponds to nSi⁄nO in the binary silicates, where nSi, nAl and nO are the ion fraction and x is a constant. The calcurated values of x were 0.90(Na2O), 0.74(PbO), 0.69(CaO) and 0.64(MnO), and the relation between their values and ion-oxygen attraction of each oxide was linear.