Kinetic model for reduction of iron oxide in molten slags by iron‐carbon melt

Amitava Paul, Brahma Deo, N. Sathyamurthy

Steel Research · 1994 · 17 citations · 4 references

Concepts

Abstract

Rate of reduction of iron oxide in iron and steelmaking slags by mass contents of dissolved carbon (>3%) in molten iron depends upon activity of FeO, temperature, mixing of bulk slag and other experimental conditions. A general kinetic model is developed by considering mass transfer of FeO in slag, chemical reaction at gas‐metal interface and chemical reaction at gas‐slag interface, respectively, as the three rate controlling steps. A critical analysis of the experimental data reported in literature has been done. It is shown that in the case of slags containing mass contents of less than 5% FeO, the reduction of FeO is controlled by mass transfer of FeO in slag plus chemical reaction at gas‐metal interface; when slags contain more than 40% FeO, the reduction of FeO is controlled by chemical reaction at gas‐metal interface plus chemical reaction at gas‐slag interface; at intermediate FeO mass contents (between ∼ 5 and 40% FeO), the reduction of FeO is controlled by all three steps, namely, mass transfer of FeO in slag, chemical reaction at gas‐metal interface and chemical reaction at gas‐slag interface. The temperature dependence of rate constant for the gas‐slag reaction is obtained as: In k 2 = –32345.4(&6128)/ T + 19.0(&3.42); σ ln k 2,1/ T = &0.3. where k 2 is expressed in mol m ‐2 s ‐1 bar ‐1 . The mass transfer coefficient of iron oxide in bulk slag is found to vary in the range 1.5 × 10 ‐5 to 5.0 × 10 ‐5 m/s, depending upon the slag composition as well as experimental conditions.

References

4