Steel Research · 1997 · 41 citations · 12 references
Materials EngineeringMaterials ScienceChemical EngineeringSurface AreaEngineeringCorrosionSurface ScienceVarious 2¼Metallurgical ProcessO AtmospheresHigh Strength Low Alloy SteelMetal DustingSurface ProcessingMicrostructureMetal Processing
The metal dusting resistance of various 2¼ Cr to 20%Cr steels has been tested in flowing CO‐H 2 ‐H 2 O atmospheres at 525, 560, 600 and 650°C. For the 2¼Cr‐steel immediately a constant rate of metal wastage is reached, for the high alloy steels the approach to this rate where all surface area is attacked, is more or less retarded by an oxide layer. The formation of a protective Cr‐rich oxide layer is favoured by a high Cr‐content of the steels, by the ferritic structure, by a fine‐grained microstructure, by surface working and by high temperatures – these factors hinder or suppress metal dusting, whereas low Cr‐concentration, austenitic structure, coarse‐grained microstructure, removal of surface deformation by etching and a critical temperature of ≤ 600°C accelerate and enhance metal dusting.
12
J. C. Nava Paz, H. J. Grabke · Oxidation of Metals · 1993 · 130 citations
H. J. Grabke, Irene Wolf · Materials Science and Engineering · 1987 · 126 citations