DentistryDental Materials ScienceOral Health SciencesDental MaterialsPreventive Dental MaterialsSurface Properties Of Dental MaterialsComposite ResinsDental CompositesBrushingCharacterization Of Composite ResinComposite Resin Surface CharacteristicsSurface Roughness EvolutionSurface Roughness ParametersSurface Smoothness EvaluationToothbrushing BehaviorToothbrushing Duration
BACKGROUND: The aim of the study was to evaluate, in vitro, the surface roughness of two composite resins submitted to simulated toothbrushing with three different dentifrices. MATERIALS AND METHODS: Totally, 36 samples of Z350XT and 36 samples of Empress Direct were built and randomly divided into three groups (n = 12) according to the dentifrice used (Oral-B Pro-Health Whitening [OBW], Colgate Sensitive Pro-Relief [CS], Colgate Total Clean Mint 12 [CT12]). The samples were submitted to 5,000, 10,000 or 20,000 cycles of simulated toothbrushing. After each simulated period, the surface roughness of the samples was measured using a roughness tester. RESULTS: According to three-way analysis of variance, dentifrice (P = 0.044) and brushing time (P = 0.000) were significant. The composite resin was not significant (P = 0.381) and the interaction among the factors was not significant (P > 0.05). The mean values of the surface roughness (µm) followed by the same letter represent no statistical difference by Tukey's post-hoc test (P <0.05): Dentifrice: CT12 = 0.269(a); CS Pro- Relief = 0.300(ab); OBW = 0.390(b). Brushing time: Baseline = 0,046ª; 5,000 cycles = 0.297(b); 10,000 cycles = 0.354(b); 20,000 cycles = 0.584(c). CONCLUSION: Z350 XT and Empress Direct presented similar surface roughness after all cycles of simulated toothbrushing. The higher the brushing time, the higher the surface roughness of composite resins. The dentifrice OBW caused a higher surface roughness in both composite resins.
15