Journal of the Ceramic Society of Japan · 1991 · 12 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMechanical Behavior Of MaterialsCeramic TechnologyFracture ResistanceFracture ToughnessStrength Of MaterialsStrength PropertiesStructural CeramicsBendingBending StrengthCeramic GlazingCeramic Material PropertiesCompressive StrengthMechanical Strength TestingPorcelain FracturePore Size Effects
The bending strength of commercial porcelains for tablewares from ten makers in Tono district, Gifiprefecture was investigated by using test bars of the same size, non-glazed or glazed and fired in respective makers. An unglazed porcelain body which showed the maximum mean bending strength of 8.9kg/mm2 had a maximum relative density of 97.5% with pore size less than 20μm. The bending strength of unglazed bodies was in the range from 4.9 to 8.9kg/mm2 and was increased to the range from 7.0 to 12.0kg/mm2 by glazing. In general, when the compressive stress in glaze was over 2.0kg/mm2, fracture occurred from the origin in the bodies and the glazing increased the bending strength of porcelain bodies by about 3.5kg/mm2. Especially, pores at the boundaries between glaze and body generated during firing acted as fracture origins and reduced the bending strength.