Preparation of High-Strength Coke by Carbonization of Hot-Briquetted Victorian Brown Coal

Aska Mori, Sousuke Kubo, Shinji Kudo, Koyo Norinaga, Tetsuya Kanai, Hideyuki Aoki, Jun‐ichiro Hayashi

Energy & Fuels · 2011 · 35 citations · 20 references

Concepts

Abstract

Cokes with tensile strengths of 6–37 MPa were prepared by binderless briquetting and subsequent carbonization up to 900 °C of pulverized Victorian brown coal that had little fluidity and very low reflectance. Application of mechanical pressures of 64–128 MPa at temperatures of 130–200 °C caused softening of the coal because of mobilization of both low- and high-molecular-mass components, deformation of the coal matrix, and then coalescence/bonding of particles. The resulting coke had a density as high as 1.1–1.3 g/cm 3 and tensile strength of 28–37 MPa, which was 5–6 times that of conventional metallurgical coke.

References

20