The Journal of Physical Chemistry C · 2011 · 208 citations · 97 references
Natural SciencesMaterials EngineeringMaterials ScienceCrystal StructureMagnetic MaterialsMaterials ChemistryAlloysFerromagnetic MaterialsFerromagnetismMagnetic Properties Of SolidsMagnetism In SolidsMagnetism Of Inorganic CompoundsCoercivityCoercivity EnhancementDendritic MorphologyMagnetic CoercivityMagnetic PropertiesNickel AlloysNickel-based AlloysSaturation Magnetization
Dendritic Ni 33.8 Co 66.2 alloy microstructures with hexagonal closed-packed phase have been prepared in large-scale by a simple and facile solution phase chemical route, while flowerlike Ni 33.4 Co 66.6 in size of 2.5–5.5 μm was synthesized by solvothermal routes. Experimental results show that the reaction temperature, total concentration of [Ni 2+ ] + [Co 2+ ], and kinds of solvent and surfactants are key factors for controlling the morphology and crystal phase of the NiCo alloy. The possible formation mechanism for the Ni 33.8 Co 66.2 dendrites has been discussed. Magnetic measurements revealed that both of the NiCo 2 alloys obtained are ferromagnetic at room temperature. The saturation magnetization value of the Ni 33.8 Co 66.2 dendrites (163.55 emu/g) is lower than that of the flowerlike Ni 33.4 Co 66.6 (195.79 emu/g), but the Ni 33.8 Co 66.2 dendritic structures exhibit an enhanced coercivity value. NiCo 2 alloys with different shapes (Ni 33.8 Co 66.2 dendrites and flowerlike Ni 33.4 Co 66.6 ) have been used as reusable heterogeneous catalysts to reduce 4-nitrophenol (4-NP) into 4-aminophenol (4-AP) by NaBH 4 . The kinetic data indicate that Ni 33.8 Co 66.2 dendrites are catalytically more active than the flowerlike Ni 33.4 Co 66.6 probably due to its larger surface-to-volume ratio and surface areas, since their Brunauer–Emmett–Teller surface areas are 32.68 and 20.66 m 2 /g, respectively.
97
Scaling of Kinetically Growing Clusters
M. Kolb, Robert Botet, R. Jullien · Physical Review Letters · 1983 · 1.1K citations