Study of the system CaO~Al2O3~H2O at temperatures of 21 degrees and 90 degrees C

L.S. Wells, W.F. Clarke, Howard F. McMurdie

Journal of research of the National Bureau of Standards · 1943 · 51 citations · 0 references

DOIFull text

Open access

Concepts

Abstract

A study has been made of the system CaO-AhOa-H20 at temperatures of 21 0 and 90 0 C. Diagrams have been constructed showing the solubility relations of the various phases at these temperatures. The solid phases were investigated by petrographical and X-ray diffraction methods. By means of X-ray diffraction patterns, it was found that the so-called hexagonal tricalcium aluminate hydrate is in reality a mixture of hexagonal 2CaO.AhOa.8H20 and hexagonal 4CaO.AhOa.13H20 intercrystallized in equimolecular proportions. On standing at room temperature, dry dicalcium aluminate hydrate is slowly converted into the tetra calcium aluminate hydrate and hydrated alumina. Loss of water of hydration in the tetracalcium aluminate hydrate results in a decrease in the unit cell along the c axis. Although the hexagonal di-and tetracalcium aluminate hydrates exist only as metastable phases in the system between 21 0 and 90 0 C, their approximate solubility relationships were ascertained at 21 0 C. As the temperature increases, the hexagonal aluminates become less stable. The only stable phases that occur in the system CaO-AhOa-H20 at atmospheric pressure over the temperature range of 21 0 to 90 0 C are gibbsite (AbOa.3H20), the isometric tricalcium aluminate hexahydrate (3CaO.AbOa.6H20), and Ca(OH)2. The solubility curves of these three stable phases in the system CaO-AhOa-H20 were determined at 21 0 and 90 0 C. Over this temperature range, gibbsite is the stable phase up to a concentration of 0.33 g of CaO pcr liter; at concentrations greater than this, 3CaO.AhOa.6H20 is the stable phase until those points are reached at which Ca(OHh also appears as a solid phase. The series of invariant points for gibbsite and the isometric phase occur at a concentration of 0.33 g of CaO pel' liter, but with the concentration of AhOa increasing from 0.02 g of Al20 a peI" liter at 21 0 C to 0.11 g of AbOa per liter at 90 0 C.