EngineeringChemical EngineeringChemistryElemental AnalysisInorganic ChemistryMetallurgyExtractive MetallurgyHeavy Metal RemovalHydrometallurgical ProcessingNutrient LeachingLeachingLeaching KineticsLeaching OptimizationLeaching ProcessesMetal LeachingOptimal Temperature RangePressure LeachingZinc Extraction
Hydrometallurgical pressure processing of EAF steelmaking dusts (by Paul Wurth S.A., Luxembourg) is investigated on a laboratory scale in the temperature range of 100 to 250 °C. The behaviour of zinc, iron and calcium under the influence of sulphuric acid as the leaching agent is discussed. The effect of temperature/pressure on the yield of the Zn-extraction is small. Only a relative small increase of pressure up to 4,1 bar at 150 °C shows some effect. The increase of temperature/pressure decreases the iron yield in a prepared solution. The concentration of H2SO4 is the most important factor for the increase of the Zn-extraction. After one or two days, the calcium sulphate generated in the solution is precipitated during the cooling of the solutions that were leached under ambient conditions. This does not apply to solutions obtained by leaching at higher temperatures/pressures. In regard to the selectivity of leaching, the optimal parameters are: T = 150 °C, c = 0.4 mol/dm 3 H2SO4 and an agitating speed of 700 rpm.
5