Thermal Stability and Mechanical Characteristics of Densified Ti<sub>3</sub>AlC<sub>2</sub>-Based Material

T. A. Prikhna, Tetyana Basyuk, Andriy Ivasyshyn, M. G. Loshak, Viktoriya Podgurska, Viktor Moshchil, Thierry Cabioc’h, Patrick Chartier, M. V. Karpets, Valeriy Kovylaev,

Diffusion and defect data, solid state data. Part B, Solid state phenomena/Solid state phenomena · 2015 · 14 citations · 2 references

Concepts

Abstract

The mechanical properties and temperature stability in air and hydrogen of the highly dense (ρ=4.27 g/cm 3 , porosity 1 %) material based on nanolaminated MAX phase Ti 3 AlC 2 (89 % Ti 3 AlC 2 , 6 % TiC, 5 % Al 2 O 3 ) manufactured by hot pressing (at 30 MPa) have been investigated. At room temperature the samples exhibited microhardness H V = 4.6 GPa (at 5 N), hardness HV50 = 630 MPa (at 50 N ) and HRA=70 (at 600 N), Young modulus was 140 ± 29 GPa, fracture toughness K 1C =10.2 MPa·m 0.5 compression strength 700 MPa and bending strength 500 MPa. After 1000 hours of exposition at 600 °C the oxide film (containing mainly Al 2 O 3 and TiO 2 ) formed on the surface and material demonstrated a higher oxidation resistance than chromium ferrite steels. Due to the surface oxidation the defects self-healing took place and the bending strength of the porous Ti 3 AlC 2 (22% porosity) after exposition for 3 h at 600 o C in air slightly (for 3%) increased as compared to that at 20 o C. Besides, the porous Ti 3 AlC 2 material resisted to high-temperature creep and after being kept in H 2 at 600 °C for 3h its bending strength reduced by 5 %.

References

2